Chris:
The Oko Institute report is available on the Europa website. They said the
key difference to the HP request was the EMI shielding. Heavy yellow
chromates used to protect bare metal are used in all categories, so that
can't be the reason they granted the exemption just for Category 3. And
trivalent chromium formulas do not work as well in bare metal protection as
hexavalent chromium coatings.
Tim
----- Original Message -----
From: "James, Chris" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Wednesday, November 01, 2006 4:46 AM
Subject: Re: [LF] Official release of the new exemptions
I agree with your sentiments but I think the judgement was made on the
corrosive resistance class of plating - new Cr3 versions are sufficient
for many domestic and internally used products whereas there is no real
substitute for the heavier and more corrosive resistant Cr6 plating
conversions required by exterior used products (these conversions are in
any case less conductive also!).
Regards,
Chris
-----Original Message-----
From: Leadfree [mailto:[log in to unmask]] On Behalf Of Timothy McGrady
Sent: 01 November 2006 09:31
To: [log in to unmask]
Subject: Re: [LF] Official release of the new exemptions
Question for all about the hexavalent chromium exemption for corrosion
resistance and EMI shielding for IT and Telecommunications equipment: I
may
be wrong, but aren't there many products which require EMI shielding per
FCC
and EU regulations falling outside the scope of Category 3 (IT and
Telecon
equipment)? Are there not applications outside Category 3 where
hexavalent
chromium coatings are used and are necessary to allow electrical contact
for
EMI shielding and corrosion resistance? I think that exemption was
lobbied
to too narrow a scope. For example, wouldn't a TV have to meet the same
EMI
shielding requirements?
Tim McGrady
----- Original Message -----
From: "John Burke" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Wednesday, November 01, 2006 3:35 AM
Subject: [LF] Official release of the new exemptions
>I placed on the blog, details of the OFFICIAL release of the exemptions
> which just got squeezed in by the TAC days before the July 1 deadline.
> They
> are now official.
>
>
>
> Link is here:
>
>
>
> http://www.rohsusa.com/blog/
>
>
>
> Kind regards,
>
>
>
> John
>
> _____
>
> From: John Burke [mailto:[log in to unmask]]
> Sent: Friday, October 13, 2006 3:32 PM
> To: [log in to unmask]; Leadfree; TechNet
> Subject: Chinese Government Delegation Coming to US to Explain New
> Environmental Regulations Impacting the High-Tech Industry
>
>
>
> A delegation of eleven high-ranking Chinese government officials from
the
> Ministry of Information Industries is coming to the US. to discuss the
> requirements of China RoHS.
>
>
>
> There is only one public event - a public seminar hosted by AeA. at
Santa
> Clara on October 26 from 7:30 am to 12:00 pm at the AeA office in the
> Techmart Building, 5201 Great America Parkway #400, Santa Clara, CA
95054.
>
>
>
> Details are here:
>
>
>
> http://tinyurl.com/yz6vog
>
>
>
> John
>
>
>
------------------------------------------------------------------------
-------Leadfee
> Mail List provided as a service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text
in
> the BODY (NOT the subject field): SIGNOFF Leadfree
> To temporarily stop/(start) delivery of Leadree for vacation breaks
send:
> SET Leadfree NOMAIL/(MAIL)
> Search previous postings at: http://listserv.ipc.org/archives
> Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at
[log in to unmask] or
> 847-615-7100 ext.2815
>
------------------------------------------------------------------------
-------
>
------------------------------------------------------------------------
-------Leadfee Mail List provided as a service by IPC using LISTSERV
1.8d
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks
send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
------------------------------------------------------------------------
-------
-----------------------------------------
This message (including any attachments) may contain confidential
information intended for a specific individual and purpose. If you
are not the intended recipient, delete this message. If you are
not the intended recipient, disclosing, copying, distributing, or
taking any action based on this message is strictly prohibited.
-------------------------------------------------------------------------------Leadfee
Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send:
SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-------------------------------------------------------------------------------
-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-------------------------------------------------------------------------------
|