Dear All,
DG Show is coming, so the reviewing meeting of IPC-T-50 is coming.
We Iook forward to see you during DG Show.
Thank you, Mr.Tong and Mr.Gong for your great support! I received so many reviewing opinions from you.
These are 7 terms which are uncertain this morning, please give us your hand. : )
Thanks and regards
Charlotte
Common Cause 共同原因 91.0229
A source of variation that affects all the individual values of the output of a process.
影响过程输出所有值的变异源。
Complex Ion 复合离子 76.0233
An ion composed of two or more ions or radicals that are capable of an independent existence.
由两个以上能独立存在的离子或自由基构成的离子。
Compliant Bond 柔性键合 74.0235
A bond that uses an elastically- and/or plastically-deformable member to impart the required energy to the lead.
采用弹性和/或塑料可变形构件将所需能量传给引线的键合。
Component Hole 元件孔 20.0238
A hole that is used for the attachment and/or electrical connection of component terminations, including pins and wires, to a printed board.
用于将元件端子固定于印制板和/或实现(与印制板的)电气连接的孔,包括插针和导线。
Component Lead 元件引线 30.1356
The solid or stranded wire or formed conductor that extends from a component to serve as a mechanical or electrical connector, or both. (See also "Component Pin.")
从元件体延伸出的实心或多股导线或成型导线,用于实现机械或电气连接,或机械/电气连接。(参见:“元件插针”。)
Component Mounting Orientation 元件安装方向 22.1357
The direction in which the components on a printed board or other assembly are lined up electrically with respect to the polarity of polarized components, with respect to one another, and/or with respect to the board outline.
印制电路板或其它组件上元件的(电气)排列方向,通常根据极性元件的极性、元件彼此之间的相互关系和/或印制板外形来排列。
Compound Die Set 复合模组合 51.1633
A set consisting of a punch and matching die used to punch holes, details or the outlines of panels and/or printed wiring boards.
由冲模和配合模组成的一套模具,用于冲孔、冲在制板和/或印制线路板的局部或整体轮廓。
|
|
|