Dear All,
These are 4 terms which are uncertain today, please give us your hand. : )
Thanks and regards
Charlotte
Bonding Wire 键合金属丝 74.0132
Fine gold or aluminum wire used for making electrical connections between lands, lead frames, and terminals.
用于在连接盘、引线框架、引线端点之间形成电气连接的细金丝或铝丝。
Bounce Pad (Discrete Wiring) 回弹垫片(分立布线) 64.1588
An isolated area in a copper plane which acts solely as a stop for the laser drilling operation.
铜面上一个只用来停止激光钻孔操作的孤立区域。
Brainstorming 头脑风暴 94.0147
The generation of an all-inclusive list of potential causal factors that are possible contributors to process problems.
列出那些可能导致流程问题的所有潜在影响因素清单的过程。
Brown Streak (Base Materials) 褐色条纹(基材) 40.1590
A thin vein or stain seen in the reinforcement that can range from light amber to nearly chocolate brown. It usually runs within a fiber bundle for 3 mm to 13 mm [0.13 in to 0.512 in]. It is most commonly found in the warp yarns and may appear singly or in multiples, or in a pattern. It is due to the remnants of the glass binder agent, which the weaver did not remove.
增强材料上可以看见的细条纹或瑕疵。颜色范围从淡黄色到巧克力色,通常出现在3mm到13mm[0.13 in -0.512 in]之间的纤维束中。最常以单个,或多个,或图案出现于经纱方向。是由于玻璃粘合剂的残余物未被清除干净引起的。
|
|
|