Sender: |
|
X-To: |
|
Date: |
Wed, 8 Nov 2006 01:28:20 +0800 |
Reply-To: |
|
Subject: |
|
MIME-Version: |
1.0 |
Content-Transfer-Encoding: |
base64 |
Content-Type: |
text/plain; charset="gb2312" |
From: |
|
Parts/Attachments: |
|
|
康来辉(讲师)
深圳市拓普达资讯有限公司
Shenzhen Toptouch Consulting Limited Company
深圳市南山区南山大道桂庙交叉路口光彩新天地13楼A1A2室
电话:0755-86196415
传真:0755-86196414
手机:13509645599
----- Original Message -----
From: "tongxm" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Wednesday, November 01, 2006 4:13 PM
Subject: Re: [TGA] Please reviewe the terms
> 校对请看附件。
>
>
> Tongxm
>
>
> ----- Original Message -----
> From: "Charlotte Hao" <[log in to unmask]>
> To: <[log in to unmask]>
> Sent: Monday, October 23, 2006 8:52 AM
> Subject: [TGA] Please reviewe the terms
>
>
>
> Dear All:
>
> Thhese the first ten terms today.Please review them and give your opinions.
>
> Least Material Condition (LMC) 最少实体情况 22.0701
>
> The condition in which a feature of size contains the least amount of material within the stated limits of size.
>
> 在规定尺寸范围内,形体包含最少实体的情况。
>
>
>
> Legend 图例 22.1439
>
> A format of letters, numbers, symbols and patterns that are used primarily to identify component locations and orientations for convenience of assembly and maintenance operations.
>
> 一种为了便于组装和维护操作所所运用的一组文字,数字,符号和图案,主要用于表征元件位置和方向。
>
>
>
> Leno End Out 末端织物脱落 44.0702
>
> Warp-end wrapper that is missing from the end of a fabric.
>
> 脱落于织物末端的弯形尾部包材
>
>
>
> Library 库 20.0706
>
> A catalog of related items that contains all of the information about the items that is necessary for processing by a computer program.
>
> 包含所有计算机程序处理相关必要信息类目的目录。
>
>
>
> Lifted Land 焊盘浮起 60.0707
>
> A land that has fully or partially separated (lifted) from the base material, whether or not any resin is lifted with the land.
>
> 焊盘与基材全部或部分分离,无论树脂是否随焊盘浮起。
>
>
>
> Lift-Off 升离 97.1905
>
> See "Solder Fillet Lifting." 参见“焊缝浮起”
>
>
>
> Light Mark (Fabric) 光标(织物) 44.0708
>
> A filling defect that extends across the width of a fabric containing less than one pick per 25 mm from nominal.
>
> 一种填充缺陷,横跨于织物的宽度方向,织物中任一梭离文字的距离不大于25毫米。
>
>
>
> Limits of Size 尺寸界限 20.0709
>
> The specified maximum and minimum sizes. 界规定的尺寸最大和最小值。
>
>
>
> Line 传输线 20.0710
>
> See "Conductor." 参见“导体”。
>
>
>
> Line Coupling 传输线耦合 21.0711
>
> The interaction between two transmission lines that is caused by their mutual inductance and the capacitance between them.
>
> 两条传输线间由于互感和互容所产生的交互作用。
>
>
>
>
>
>
> Thank you!
>
> IPC TG2-30CN Secretary:Charlotte
|
|
|