Thanks to all that have replied here.
It is actually a lot to lot variation issue on a D2PAK. They claim the issue we are having is because we are below the melt point of tin (?!!). . Agree with your gold example (I argued by using copper).
Although I couldn't see why, I wanted to be sure that there wasn't something unique to electroplating compared to hot tin dipping that I've been missing all these years. Thought I'd be opened minded towards their thoughts and ask the forum.
I'm suspecting co-deposited organics and/or problem at the Ni interface below.
Rich K
________________________________
From: TechNet on behalf of David D. Hillman
Sent: Thu 10/26/2006 7:09 AM
To: [log in to unmask]
Subject: Re: [TN] Backward Compatibility of Tin Electroplating
Hi Rich! Unless the electroplated tin has some unique surface finish
characteristics, it is not necessary to exceed 232C (the melting point of
tin) in the reflow process. Some folks don't realize that the majority of
solder connections are the result of molten solder alloys diffusing into
component or pwb surface finishes rather than both surfaces being molten.
An example I like to use is that if we needed to "melt" a gold surface
finish (which some component fabricators use as their solderable finish)
then we would need to achieve a reflow profile exceeding 1064C which would
be a bit of an issue for the rest of the assembly! Could the vendor be
suggesting that 232C needs to be exceeded for some other reason than
creating the solder joint?
Dave Hillman
Rockwell Collins
[log in to unmask]
Richard
Kraszewski
<[log in to unmask] To
COM> [log in to unmask]
Sent by: TechNet cc
<[log in to unmask]>
Subject
[TN] Backward Compatibility of Tin
10/26/2006 12:17 Electroplating
AM
Please respond to
TechNet E-Mail
Forum
<[log in to unmask]>
; Please respond
to
Richard
Kraszewski
<[log in to unmask]
COM>
Does anyone have any reason to suspect that tin electroplated SM
components being soldered with a 63/37 solder paste require a profile
that must exceed the reflow temperature of tin?
Being told by a component vendor this is the case. I would totally
discount this but seem to recall reading this more than once on some
other component Tech data sheets. I can't explain why this would be
necessary, but.....
Any thoughts would be appreciated.
Rich K / Kimball
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|