TECHNET Archives

October 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Jack Olson <[log in to unmask]>
Date:
Thu, 12 Oct 2006 16:11:05 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Dehoyos, Ramon" <[log in to unmask]>
Subject:
From:
"Dehoyos, Ramon" <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (105 lines)
        In IPC website there is a search tab. It might help you
        Ramon
 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jack Olson
Sent: Thursday, October 12, 2006 4:03 PM
To: [log in to unmask]
Subject: Re: [TN] Compression Limit on FR4?

I don't know.

That's why I wondered if there was any kind of industry consensus on the
subject.

Jack


On 10/12/06, Ian Hanna <[log in to unmask]> wrote:
>
> 'damage' occurs as soon as you assemble the board...
>
> how much 'damage' is acceptable to your application?
>
>
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Jack Olson
> Sent: Thursday, October 12, 2006 3:53 PM
> To: [log in to unmask]
> Subject: Re: [TN] Compression Limit on FR4?
>
> Thank you for responding.
>
> The problem is, someone is asking me about the MAXIMUM before damage 
> occurs, so I am quite interested in your statement that it "tends to 
> deform the fiberglass over time".
>
> Where can I learn more about that?
> Does any IPC document even mention it?
> I wish there was such a thing as an "IPC index"... any IPC people 
> listening?
>
> thanks again, though
> Jack
>
>
> On 10/12/06, Stadem, Richard D. <[log in to unmask]> wrote:
> >
> > Hi, Jack
> > I can tell you that typically the torque setting used for hardware 
> > on pwb assemblies is between 1 to 6 in/lbs. More than that tends to
> deform
> > the fiberglass over time. Of course, it all depends on the type of
> board
> > material, layer count, etc.
> > It also depends on the application.
> > Realize that a lot of relaxation occurs during any type of thermal 
> > excursion, and the hardware will loosen up. It is always a good idea
> to
> > use a Bellville washer in conjunction with a serrated or star washer
> to
> > continue to hold the torque. It is also a good idea to use Glyptol 
> > or some other threadlocker.
> >
> > -----Original Message-----
> > From: TechNet [mailto:[log in to unmask]] On Behalf Of Jack Olson
> > Sent: Thursday, October 12, 2006 1:54 PM
> > To: [log in to unmask]
> > Subject: [TN] Compression Limit on FR4?
> >
> > Does anyone know of any guidelines or recommendations that suggest a

> > maximum limit on compressing board material?
> >
> > Can any damage occur by over-torque'n screws, for example?
> >
> > I've never heard anyone discuss that...
> >
> > Jack
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2