Dear All:
These are Batch 9th terms . Please review them and give your opinions.
Hi Jason, Thank you. :)
Metal Migration 金属迁移 96.1445
The electrolytic transfer of metal ions along an electrically conductive path from one metal surface to another when an electrical potential is applied to the two metal surfaces.
当电压作用于两个金属表面时,金属离子在电解作用下通过导电通路从一金属表面迁移到另一面。
Metal Migrativity 金属迁移率 96.0754
The comparative rate of the velocity of metal migration under the same conditions.
在相同条件下金属迁移的相对速率。
Metal Surface Migration 金属表层迁移 96.1226
The migration of metal on the surface of an electrical insulator.
电子绝缘体表层的金属迁移。
Metal Through Migration 金属介质迁移 96.0662
The migration of metal through an electrical insulator.
以电子绝缘体为介质的金属迁移。
Metallized Land Areas 金属焊盘区 22.1756
A pattern of conductive material used on a substrate to interconnect electronic components. Widened conductor areas used as attachment point for wire bonding or other devices.
线路板内层用以连接电子元件的导电材料物质。用作为导线节点或其他器件辅助导电点的拓宽导电区域。
Metallization (n.) 镀金 (n.) 53.0753
A deposited or plated thin metallic film that is used for its protective and/or electrical properties.
薄金属镀层用作于电路保护和/或其他电气性能。
Microbond 微结点 74.0756
A termination made with a small diameter wire, i.e., 0.025 mm [0.001 in] or less.
以直径不大于0.025mm [0.001 in] 导线做成的结点。
Microcircuit 微电路 30.0757
A relatively high density combination of equivalent circuit elements that are interconnected so as to perform as an indivisible electronic circuit component.
互联的不能分割的高密度组合的等效电路。
Microcircuit Module 微电路模块 86.1446
A combination of microcircuits and discrete components that are interconnected so as to perform as an indivisible circuit assembly.
互联的微电路和分立元件组合成的不可分割的电路集合。
Microelectronics 微电子学 30.0759
The area of electronic technology with, or applied to, the realization of electronic systems from extremely-small electronic elements, devices or parts.
应用于实现以极微小电子元器件构成的电路系统的电子科技领域。