Steve,
Those things almost look big enough to be fishing weights! Interesting
that so much solder could spit off the board without taking components
with it. Not surprising that tombstoning could result.
Are you going into the lead-free fishing weight and tire balance weight
business on the side?
Isn't it obvious that "no one else has this problem". I hear that
all
the time with various polymers and ultralight aircraft engine
complaints.
Please keep us posted
Steve
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Tuesday, October 31, 2006 9:57 AM
To: [log in to unmask]
Subject: [TN] Bizzare Phenomena...
Mornin' All!
This morning I have seen something that I have never, ever have seen
before. It's been a little slow the past week, so we decided to do our
maintenance on our reflow ovens. After we opened the oven up, we found
many, many solderballs laying on the bottom of the oven right around
zone 7 - 8, right at the beginning of the spike zone. Check-out:
http://stevezeva.homestead.com/files/Oven_Solderballs.jpg
http://stevezeva.homestead.com/files/Oven_Solderballs_2.jpg
http://stevezeva.homestead.com/files/Oven_Solderballs_3.jpg
http://stevezeva.homestead.com/files/Oven_Solderballs_4.jpg
We've been having tombstoning problems when we've run the two lead-free
jobs that we have here. I've been working with the paste vendor sending
my profiles and plots, but I haven't been able to solve the problem. The
solderballs in the oven are lead-free solderballs.
We are using a Heller 1809, and my profile set-points are:
120 140 160 180 190 200 230 240 250
120 140 160 180 190 200 230 240 250
Belt speed 26 in per min
The paste is a SAC 305 with a water washable no-clean flux. I think my
profile is pretty reasonable, and the last board we ran is pretty
standard, .062" thick, with no bizzare copper planes. The board finish
with both jobs has been ENIG. The last job I ran we were tombstoning
0805's, the one before that we were tombstoning 0402's. With both jobs
we've had major tombstoning problems. I've slowed the beltspeed down,
sped it up, ramped up slower, ramped up faster, changed this, changed
that, but still haven't resolved my tombstoning.
Of course, I'm the only one that's having this problem according to my
paste vendor...
I wouldn't have imagined that I would see the solderballs in the oven
like we have...
Have any of you ever seen something like this before?
-Steve Gregory-
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
THE INFORMATION CONTAINED IN THIS E-MAIL MESSAGE AND ANY ATTACHMENTS SENT FROM GENTEX CORPORATION IS GENTEX CONFIDENTIAL INFORMATION INTENDED ONLY FOR THE PERSONAL USE OF THE INDIVIDUAL OR ENTITY NAMED ABOVE. If you are not the intended recipient, you are hereby notified that any review, distribution, or copying of this communication is strictly prohibited. If you have received this communication in error, please immediately notify the sender by return e-mail, and delete this e-mail message and any attachments from your computer.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|