TGASIA Archives

October 2006

TGAsia@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Transfer-Encoding:
quoted-printable
Sender:
Subject:
From:
Charlotte Hao <[log in to unmask]>
Date:
Mon, 30 Oct 2006 21:19:54 -0600
Content-Type:
text/plain; charset="gb2312"
MIME-Version:
1.0
Reply-To:
Asia Committe Task Group Forum <[log in to unmask]>, Charlotte Hao <[log in to unmask]>
Parts/Attachments:
text/plain (24 lines)
 
Dear All,
 
Today there are two terms which are uncertain, would you like to help us?
Thanks and regards 
 
Charlotte

Metal Migration                                 金属迁移                96.1445

The electrolytic transfer of metal ions along an electrically conductive path from one metal surface to another when an electrical potential is applied to the two metal surfaces.

当电压作用于两个金属表面时,金属离子在电解作用下通过电气导电通路从一金属表面迁移到另一金属表面。

 

Metallized Land Areas                     金属化焊盘区域     22.1756

A pattern of conductive material used on a substrate to interconnect electronic components. Widened conductor areas used as attachment point for wire bonding or other devices.

基板上用以实现电子元件互连的导电材料图形。加宽的导体区域用作导线绑定或其他器件的连接点。

 