Dear all,
I want to ask you the following term.
Multiple Image Production Master 24.1643
A production master having at least two 1:1 scale patterns.
What is the meaning of master?
Thanks
Charlotte
________________________________
From: Leesha Peng
Sent: 2006-10-22 (星期日) 22:48
To: John Perry; Jack Crawford
Cc: Charlotte Hao
Subject: t-50 translation
Hi All,
What does " pick and norminal " mean in this term?
Light Mark (Fabric) 44.0708
A filling defect that extends across the width of a fabric containing less than one pick per 25 mm from nominal.
PS:
You could put questions to John and Jack from HQ for T-50 translation job.
Leesha Peng 彭丽霞
技术与培训部总监
Director Technical and Training Program
IPC WOFE, a subsidiary of IPC, Inc.
爱比西国际科技管理咨询(上海)有限公司
上海市宜山路711号
Tel: 021-54973435
Fax: 021-54973437
邮编:200233
手机:13902994705
|
|
|