TECHNET Archives

October 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Fri, 20 Oct 2006 07:27:53 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Charlie McMahon <[log in to unmask]>
Subject:
From:
Charlie McMahon <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (56 lines)
Good Morning All:



Might I ask for some guidance from you all..



In determining a surface coating a conflict has arisen between choosing Gold
immersion vs. Silver immersion as the

choice. The application is for boards that are used in shipboard electronics
(non military) but they are protected from the external environment.



My question is which is the more appropriate coating?

Technically, the gold has always worked from the PCB fab and assembly end
with success with a controlled cost of ownership.

The silver however is one that causes concern.



Any suggestions would be appreciated.



Best Regards,



Charlie McMahon

McMahon Sales Company










---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2