In addition, the differences in CTE mismatch between small caps and
larger caps is so small as to be neglible. You are still "anchoring" the
caps by allowing large fillets around the three sides of the endcaps,
with little solder underneath. If the cap is a MLCCC with a ceramic body
material, then there is nothing to absorb the cyclic strains. Hence
there are going to be either the solder joint cracks, or the capacitor
itself will crack.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner Engelmaier
Sent: Thursday, October 19, 2006 7:07 AM
To: [log in to unmask]
Subject: Re: [TN] Tombstoning and nitrogen
Hi David,
What happens with all chip components and large pads is, that most of
the solder goes for the fillets and very little winds up between the
chip and the PCB pad. Thus, the stand-off height, one of the prime
reliability parameters, is very small and you get crack initiation
underneath the chip very early. What the fillets do in this case is
provide functional life because of the larger volume through which the
cracks need to propagate for functional failure. Out in the fillets the
cyclic strains are smaller than underneath the chip, because of a much
larger 'effective' solder joint thickness.
However, you would be much better of if the solder were underneath the
chip instead of the in the fillet, thus preventing any premature crack
initiation in the first place.
Werner
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|