I switch to using nitrogen about a year ago. We use two different
solder finishes on our boards HASL and ENIG. Have the same problem as
you explain. We didn't have a problem with tombstones until we stared
to use nitrogen. The benefit of N2 with increase wetting is what causes
the problem. I changed our stencils apertures for 0402's to home plate
apertures. This has a lot but we still have some occurrences. I have
also changed the land pattern and reduced the size of the pad, this has
helped a lot. The only thing left that I am going to try is adjusting
my PPM level of O2 to around 900ppm. This is supposed to help with
tombstoning but retain the benefits of N2.
Hope this helps.
Scott Lefebvre
Scott Lefebvre
-----Original Message-----
From: Gabriela Bogdan [mailto:[log in to unmask]]
Sent: Tuesday, October 17, 2006 1:53 PM
Subject: Tombstoning and nitrogen
Netters,
We recently started to use reflow under nitrogen on OSP coated boards.
These boards were previously immersion silver plated and we reflowed
them in air. Very few tombstoning was seen.
Our customer decided to change the finish and requires mandatory reflow
under nitrogen.
We are completing all the soldering operations within 2 days. We use no
clean solder paste and no clean flux.
Questions:
1. Did anybody experience increase of tombstoning of 0402 passives when
using nitrogen?
2. Is using nitrogen during reflow beneficial for the next process-
selective wave soldering under nitrogen?
3. For thick multilayer boards with more than 20 layers, can complete
hole fill be expected during wave soldering of OSP boards after double
reflow?
If you had any similar experience, could you tell me how you solved
these problems?
Thank you,
Gaby
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|