Not one single count of Cobalt.
Inge
----- Original Message -----
From: "R Sedlak" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Wednesday, October 18, 2006 1:09 AM
Subject: Re: [TN] ENIG problem
> Ingemar:
>
> I have a suspicion you may have found the answer...
> Thick gold can only mean electroplated gold... electroplated gold is often
> alloyed (think Cobalt is most common alloying metal)... which undoubtedly
> would make bonding difficult.... remember, in electroplating gold, pure
> gold is often referred to as "soft gold".... the alloying metals are
> present to harden the gold... which has to interfere with bonding...
>
> And from the comments about appearance, it may well not be well alloyed.
>
> Rudy Sedlak
> RD Chemical Company
>
> "Ingemar Hernefjord (KC/EMW)" <[log in to unmask]> wrote:
> Hi amigos,
> I should never said that we had no ENIG problems. Now we seem to have
> one. Chinese board supplier. Problems with heavy wire aluminum bonding
> on the ENIG pads. Too low pull test values. Possible reason: pad surface
> invaded by copper particles after the bake/reflow/mounting. Sending
> picture to Mr Yoda. Never seen this before. Gold is too thick for being
> ENIG (>1um), Nickel about 6um. Can't see how Copper could diffuse to the
> surface so rapidly and at those low temperatures which are typical for a
> general assembly process. Any clue? Graham? You seem to be sitting at
> the keyboard just now.
> Ingemar Hernefjord
> SAAB MICROWAVE SYSTEMS
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
>
>
> ---------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
> Get your email and more, right on the new Yahoo.com
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|