TECHNET Archives

October 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Tue, 17 Oct 2006 21:16:29 +0000
Reply-To:
Subject:
From:
Sherif Refaat <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Type:
text/plain; charset="utf-8"
Content-Transfer-Encoding:
base64
Parts/Attachments:
text/plain (1 lines)


Sherif Refaat

Sent from my BlackBerry   



-----Original Message-----

From:         Werner Engelmaier <[log in to unmask]>

Date:         Tue, 17 Oct 2006 17:05:12 

To:[log in to unmask]

Subject: Re: [TN] ENIG problem



Hi All,

I doubt very much this is ENIG—they must have simply substituted ED Au for 

the iAu—that is what happened in my situation.



Werner



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 1.8e

To unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest

Search the archives of previous posts at: http://listserv.ipc.org/archives

Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815

-----------------------------------------------------


ATOM RSS1 RSS2