TECHNET Archives

October 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Saint Jerky <[log in to unmask]>
Date:
Mon, 2 Oct 2006 20:44:42 -0500
X-To:
"R. Dean Stadem" <[log in to unmask]>
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Saint Jerky <[log in to unmask]>
Parts/Attachments:
text/plain (79 lines)
haha..I am a HE.  Thanks guys for sharing your view. Based on so many
contributions, can I conclude that the paint is splash prior to the Mounting
process? As for who create it, both the supp & cust have suspicious as the
paint could have inhere "after supp completed their fluxing process" and
"prior to customer Mounting" process since the paint is splash over the
those patterns(Resist & Silk print)surface.

As for some of the paint seem to be under the pattern, I think maybe is due
to the photo not showing lighter orange tone well thus making it look like
it disappear. As I can see majority of the paints is covering over the board
surface.

Anyway, the evident is already gone as supp already washed off the paint
when they do a reflux on the board.

On Mon, 2 Oct 2006 12:49:44 -0500, Stadem, Richard D.
<[log in to unmask]> wrote:

Dear Mr.  (Ms?) Jerky, If you look closely, you can see evidence of the
"paint" or discoloration only on some of the pads and along some of the
traces, but not on the soldermask area around it.  It also appears to have
blocked the etching process, leaving etching flaws between the traces,
especially those on the left side of the image.  I say appears, because they
may not be copper bridges, but paint bridges.  But based on the fact that
none of the paint appears on the board surrounding certain pads but is
covering those pads, it has to be a problem that originated during
fabrication of the pwb.
On the other hand, there are areas of solder mask covered with the paint.
It is hard to judge from the picture, but is it possible that you have two
problems, one being a poor plating process, the other splattered paint from
some other process during assembly or fabrication?  I think some of the
orange in the picture is unplated copper, some orange that is a slightly
darker shade is paint.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of John Burke Sent: Monday,
October 02, 2006 12:14 PM To: [log in to unmask] Subject: Re: [TN] Customer or
Supplier Inherent Defect?  Share your views

There are indications that the paint was on the board prior to solder paste
and reflow.

John


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Saint Jerky Sent:
Monday, October 02, 2006 4:49 AM To: [log in to unmask] Subject: [TN] Customer
or Supplier Inherent Defect?  Share your views I encounter 1pcs of excess
paint on PCB returned from customer.
Upon analysis by Supplier, they concluded that customer created the defect.
The details is as below:
Defect: Paint spread over the PCB Analysis:
1) The affected surface was subjected to the fluxing process again and the
stain was found to be removed from the process.
2) The stain is unlikely to have been incurred during the bare board
processing, as fluxing process is conducted just before Final Inspection and
Packing,
3) If the stain is incurred during the bare board processing, it will have
been cleaned up during the fluxing process prior to inspection.
4) Final Inspection and packing does not uses any material that yield such a
colour substance
Photo: http://img242.imageshack.us/img242/7362/bareboardzd6.jpg
Based on the photo, tell me what you guys think?
The chances that customer created it is higher or supplier?  Come and share
your views for my reference.  Thanks.

---------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2