TECHNET Archives

October 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Hfjord <[log in to unmask]>
Date:
Mon, 16 Oct 2006 10:07:44 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, John Burke <[log in to unmask]>
Subject:
From:
John Burke <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
<006d01c6f144$b14e32c0$6501a8c0@compaq>
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (128 lines)
Looks like gold, feels like gold, sounds like gold when running the fingers
through large heaps of coin........Ahhhhhhhhhhhhhhh

Oooops sorry,

Got carried away there............8-)

Late Friday moment,

John

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Hfjord
Sent: Monday, October 16, 2006 10:01 AM
To: [log in to unmask]
Subject: Re: [TN] Suspect PCBs

reminds of a problem we had once: there was no nickel at all under the gold,
XRF or EDAX will tell you. Also, we have seen 'dull gold' from a chinese
supplier. In that case there was nearly no gold present, so what we saw was
nickel. Again, agree with the others, don't wait, make a XRF or EDAX.
Wouldn't listen to the explanations given, gold is gold, and should look
like gold. Amen.
Inge



----- Original Message -----
From: "Tom Parkinson" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Monday, October 16, 2006 3:47 PM
Subject: [TN] Suspect PCBs


Hello All (DN & TN),

I'm having a disagreement with one of my board vendors.  We have rejected
some of the boards for "suspect bad pads" (ENIG).  During visual inspection,
the suspect pads 'jump out' at you by looking dark in color.  At the very
least, they sure refract the light the wrong way making them look dark in
color. Rotating the board does not make them look better.

In the past we have tried soldering to these pads and have run into problems
with wetting.  In my letter to the vendor, I mentioned the ENIG was either
too thick, or too thin, both which will cause problems.

I'm especially worried about these when they are under BGAs.

The vendor says there is nothing wrong with the pads as-is.  In fact he said
the following:

=========================
"Boards are good.  There is no black Pad - only dull gold.  Xxxxxx (board
vendor) is "Cleaning" the gold to make it look "Pretty".  We will be
returning the boards on Monday to you.

There is always a variation in surface color with any immersion gold
process. It may be minimal in some cases or more obvious as in the boards in
question. But problem is not the correct description, variation is the
correct term. It will not effect form fit or function.

The color variation you refer to is not because of the variation in
thickness. Three to seven micro-inches of gold is deposited over 100 to 150
micro-inches of nickel. The gold vaporizes during your reflow process and
the adhesion is solder to nickel. There will be no adherence problem. By the
same token, there is no embrittlement problem with immersion gold as there
would be with electro-plated gold. For one thing electro-plated gold is 10
times thicker than immersion gold. Secondly the grain structure of immersion
gold and electro-plated gold is very different. Electro-plated gold having a
long grain structure in comparison to immersion gold.

Using a pencil eraser as you suggest only proves my point. The surface color
variation is caused by an alkaline deposit on the surface of the gold which
vaporizes on contact with molten solder. We propose to clean the boards
using a mild baking soda solution."
==========================

Looking forward to your inputs.

Thanks,

Tom



Tom Parkinson
Quality System Manager - CIT
WinTronics, Inc.
Phone: 724-981-5770 - extension 235

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2