TECHNET Archives

October 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Mon, 16 Oct 2006 10:26:28 EDT
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="UTF-8"
From:
Werner Engelmaier <[log in to unmask]>
Parts/Attachments:
text/plain (31 lines)
Hi Tom,
Your PCB vendor is giving you a mish-mash of correct statements and technical 
nonsense.
>>The gold vaporizes during your reflow process and the adhesion is solder to 
nickel.
A: this is absolute nonsense—the Au disolves very quickly in the Sn of the 
solder.

>>By the same token, there is no embrittlement problem with immersion gold as 
there would be with electro-plated gold.
A: Correct.

>>Secondly the grain structure of immersion gold and electro-plated gold is 
very different. Electro-plated gold having a long grain structure in comparison 
to immersion gold.
A: this is absolute nonsense—certainly, iAu and eAu have different structures 
as plated, but what difference does this make once the disolve to form SnAu 
IMCs.

Werner

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2