Had you placed any sticky labels etc onto the assembly before
fluxing/soldering. It seems like something has flowed or blown over the
surface.
I would also be concerned about the amount of delamination noted on the
panel edged - it's a multilayer PWB! Ingress of moisture etc could cause
issues later.
Colin McVean M.Inst.C.T.
Production Manager
Artetch Circuits Limited
Main: 01903 725365
DD: 01903 712926
Email: [log in to unmask]
www.artetch.co.uk
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dan Mauro
Sent: 02 October 2006 13:06
To: [log in to unmask]
Subject: Re: [TN] Customer or Supplier Inherent Defect? Share your views
I think it is interesting that no paint is present on any components
from what I can see.. That tells me it is supplier and/or your
operation created it!
Dan Mauro
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Saint Jerky
Sent: Monday, October 02, 2006 7:49 AM
To: [log in to unmask]
Subject: [TN] Customer or Supplier Inherent Defect? Share your views
I encounter 1pcs of excess paint on PCB returned from customer.
Upon analysis by Supplier, they concluded that customer created the
defect.
The details is as below:
Defect: Paint spread over the PCB
Analysis:
1) The affected surface was subjected to the fluxing process again and
the
stain was found to be removed from the process.
2) The stain is unlikely to have been incurred during the bare board
processing, as fluxing process is conducted just before Final Inspection
and Packing,
3) If the stain is incurred during the bare board processing, it will
have
been cleaned up during the fluxing process prior to inspection.
4) Final Inspection and packing does not uses any material that yield
such
a colour substance
Photo: http://img242.imageshack.us/img242/7362/bareboardzd6.jpg
Based on the photo, tell me what you guys think? The chances that
customer
created it is higher or supplier? Come and share your views for my
reference. Thanks.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|