Hi, Jack
I can tell you that typically the torque setting used for hardware on
pwb assemblies is between 1 to 6 in/lbs. More than that tends to deform
the fiberglass over time. Of course, it all depends on the type of board
material, layer count, etc.
It also depends on the application.
Realize that a lot of relaxation occurs during any type of thermal
excursion, and the hardware will loosen up. It is always a good idea to
use a Bellville washer in conjunction with a serrated or star washer to
continue to hold the torque. It is also a good idea to use Glyptol or
some other threadlocker.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jack Olson
Sent: Thursday, October 12, 2006 1:54 PM
To: [log in to unmask]
Subject: [TN] Compression Limit on FR4?
Does anyone know of any guidelines or recommendations that suggest a
maximum limit on compressing board material?
Can any damage occur by over-torque'n screws, for example?
I've never heard anyone discuss that...
Jack
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|