Bob,
Lot's of things to try here..
- Try baking both the PCB and the component prior to soldering. You need to
check the temperature limitations of your other components and also the
transformer (plastic bobbin?) for the appropriate temperature to bake at.
Common temp to pre-bake is in the 200 to 250F range.
- You can also heat from the top side while soldering with a heat bath.
Check a company called Zephyrtronics. They make temperature controlled heat
baths.
- You did not state is what your iron temperature is, but you may be able to
increase that temperature?
- Review the iron tip size. Is the tip sized properly to maximize your heat
flow? Use the widest tip possible to cover but not exceed the contact area,
and a shorter tip recovers faster (shorter heat path).
- You can also increase the wattage of the soldering iron. 80-85W should
work for most ground planes if substrates are preheated..
Lastly, this is an obvious one, make sure there is good solderability of the
component and PCB....
Good luck.
Kevin Glidden
Manufacturing Engineer
Astronics Luminescent Systems Inc.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bob Arciolla
Sent: Tuesday, October 10, 2006 1:44 PM
To: [log in to unmask]
Subject: [TN] vertical fill problem
Good afternoon,
I have a situation where I have a transformer that I am populating in a pcb
and I have a ground plane right up next to it and between the ground plane
and the core of the transformer, I cannot meet the IPC requirement of 75%
vertical fill on the tranformer leads. Any suggestions?
Thanks in advance,
Bob Arciolla
Endicott Research Group
Quality/Safety Manager
607 754-9187 ex 3034
607 754-9255 fax
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
cell 607 624-8516
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|