We are not allowed to have more than 500 Volts between surface traces and
layers below . Over 500 Volts, FR-4 is not used because of the humidity
risks, also high altitude phenomenons, like corona effects. For 1500 Volts
we would typically use PTFE 1500 Volts means a high activation and the
board is therefore much more susceptible to migration and other high voltage
driven disasters. The dielectric withstanding is expressed in kV/mm, e.g. 40
kV/mm, and it makes people think kV rather than Volts. I represent HiRel and
Mil manufacturing, I can imagine that the home electric equipment industry,
and other commercials, have a less stringent desing rule here.
Inge
----- Original Message -----
From: "Wayne Thayer" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Monday, September 25, 2006 11:41 PM
Subject: Re: [TN] High-Voltage Board Spacings
> Your failure mode of deepest concern is most likely CAF (Conductive
> Anodic Filament). The most common spot for this problem is via to
> trace, and the seed is disturbances in the via side wall. CAF can also
> grow along glass filaments within pre-preg from layer to layer. Failure
> potentials are at less than 10% of the 750V/mil. Laminates are
> available with very high CAF resistance if you need to push things. I
> believe there are some BT based materials that are virtually immune, but
> 1500V is a lot of potential!
>
> Wayne Thayer
>
>>>> [log in to unmask] 9/25/2006 5:06 pm >>>
> Should I be using IPC Table 6.1 for conductor spacing for high voltage
> in the z-axis of the pcb?
> Or should I be using the approximately 750V/mil spec from the laminate
> supplier and derate that number?
> Board has +/- 1200V.
>
> Thank you.
>
> Kaye Clayo
> Sr. P. C. Layout Designer
> Keithley Instruments, Inc.
> 440-498-2862
>
> CONFIDENTIALITY NOTE: This message is intended only for the use of the
> individual or entity to which it is addressed and may contain
> information that is privileged, confidential, and exempt from disclosure
> under applicable law. If the reader of this notice is not the intended
> recipient, you are hereby notified that any dissemination, distribution
> or copying of this communication is strictly prohibited. If you have
> received this communication in error, please notify the sender
> immediately.
>
>
>
> _____________________________________________________________________________
> Scanned by IBM Email Security Management Services powered by
> MessageLabs. For more information please visit http://www.ers.ibm.com
> _____________________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text
> in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
> ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|