If the washer is conductive, and, is within .00512" from the trace then you
violate the requirements of the design spec. You might also have UL
requirements to consider.
Franklin
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Abel, Shannon K.
Sent: Thursday, September 21, 2006 10:13 AM
To: [log in to unmask]
Subject: Re: [TN] Mechanical Hardware Clearance...
It is relavent when my PM is asking. While I know its not best practice, I
need to find what the correct answer is.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Whittaker, Dewey
(EHCOE)
Sent: Thursday, September 21, 2006 11:01 AM
To: [log in to unmask]
Subject: Re: [TN] Mechanical Hardware Clearance...
IMHO
It is irrelevant whether you violated any guideline or not. Do not ever
mount any conductive entity over a trace which then relies solely on the SM
for electrical protection.
Dewey
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Abel, Shannon K.
Sent: Thursday, September 21, 2006 7:44 AM
To: [log in to unmask]
Subject: [TN] Mechanical Hardware Clearance...
I have a board with a 15VDC trace on the surface layer that runs under a
flat washer.
The trace is covered by SM, which provides 500vdc isolation per .001 mil of
SM coating.
2221 states that any electrical conduction trace per sec 6.3 lists a minimum
clearance of .00512 to any other conductive surface (.ie mechanical
hardware)
Do I violate the spec.
Any help would be greatly appreciated.
Shannon Abel
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per
day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information,
or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please visit
IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|