AAAAAAAAAAAAAAAAAArggggggggggghhhhhhhhhhhhhhhh
It depends............
BUT from what you describe I would check the finish on the BGA substrate, I
have seen this a few times on enig BGA substrates caused by stress in
cooling down from reflow temperatures.
The reason for the corners is maximum stress due to longest length on
diagonal.
John
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Rudolph yu
Sent: Friday, September 15, 2006 11:22 AM
To: [log in to unmask]
Subject: [TN] Need help on a Dye & Pry test result
Recently I asked an outside lab to perform the dye & pry test on couple
failure assemblies. The heatsink was not removed from the PBGA prior to the
dye application.
According to the result and pictures, the corner pads of the BGA package
from both units were covered by the dye completely . An indication that a
seperation was formed between the BGA package's pads and its original solder
balls at that one corner after the SMT process.
Have anyone of you experienced this kind of defects in the past and what
could be the root cause of this phenomena? ( Poor plating from the IC
manufacturer? SMT reflow profile? PCB warpage? )
I have been in the industry for 10 years and have never seen thing like
this. Is it common??
Thanks
Ryu
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|