Hi Helena:
Laminates are insulators and prevent arcing
between two conductors. Separation of laminates or " Delamination" may
allow two conductors to be separated by air instead. Air is not as good
insulator as fiber glass/epoxy laminates or other materials. So
delamination may allow arcing between two traces or pads, which may burn
the board. Short version. See IPC-A-610D section 10.2 Laminate
conditions
Regards,
Ramon
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Pasquito, Helena
Sent: Tuesday, September 12, 2006 12:45 PM
To: [log in to unmask]
Subject: [TN] Delamination
Hi TechNetters,
Let me ask a question; I know delamination is bad, but why? What is the
failure mode to the board when a board delaminates and would there ever
be an instance that a board that delaminates is still OK to use? This
is a Class 3 application. Yes, I know what the IPC standards say but
not real sure about the board process. Yes, I "googled" and there is a
lot of stuff out there. Maybe someone can recommend some reading
material (hopefully short and sweet and to the point).
Thanks!
Helena
Helena Pasquito
Manufacturing Skills Instructor
M/A-COM, Tyco Electronics
1011 Pawtucket Blvd., M/S 107
Lowell, MA 01853
978-442-5024
[log in to unmask]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|