Sorry, but a) what plastic b) what contaminants are you trying to remove
c) why are you sing ultrasound d) what additives, if any, are added to
the water e) what temperature and f) what characteristics of ultrasound?
Depending on the nature of the plastic, IPA may cause stress-cracking.
Brian
Eric CHRISTISON wrote:
> We're currently ultrasonically cleaning some plastic parts in DI water
> and may be incurring some microscopic damage to the surface.
>
> We've been directed to use IPA rather than DI water as a cleaning medium
> to give a gentler clean to reduce damage.
>
> Does this sound like a good plan and would there be any other fluids
> that would be more suitable?
>
> Regards,
>
>
> --
> Eric Christison Msc
> Mechanical Engineer
> Home Personal, Communication Sector
> Imaging Division
>
> STMicroelectronics (R&D) Ltd
> 33 Pinkhill
> Edinburgh EH12 7BF
> United Kingdom
>
> Tel: +44 (0)131 336 6165
> Fax: + 44 (0)131 336 6001
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
> ext.2815
> -----------------------------------------------------
>
--
http://www.cypenv.org Cyprus environment/energy
http://www.cypenv.org/worldenv World environment/energy
http://www.cypenv.org/weather Cyprus weather
http://www.cypenv.org/smf/index.php Environment/energy forums
http://groups.yahoo.com/group/cypnature/ Cyprus nature forum
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|