TECHNET Archives

September 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Mon, 25 Sep 2006 07:50:14 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Tempea, Ioan" <[log in to unmask]>
Subject:
From:
"Tempea, Ioan" <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (50 lines)
Keith, Karl, Dave,

thanks, it is very clear. Scientific explanation, exactly what I hoped for. Now I can justify filling the rework mini-wave with SN100C.

May thanks,

Ioan

-----Original Message-----
From: Leadfree [mailto:[log in to unmask]]On Behalf Of MA/NY DDave
Sent: Sunday, September 24, 2006 1:45 AM
To: [log in to unmask]
Subject: Re: [LF] FW: [TN] Dissolving copper hole wall using lead free
HASL?


Hi Again KeithS, Karl, Ioan, IPC LF Listservers,

Forgot to add something

<So in a process like HASL, or Wave, which continually washes fresh solder
past the interface the Cu6Sn5 which is formed is washed away and more Cu is
dissolved by the Sn until the washing away stops.>

Since the solder serves a dual purpose of bring the entire component lead
and the entire board at each hole interface up to temperature we need to
keep it in the process long enough, which increases the dissolution rate
for certain hole/lead interfaces.

Yours in Engineering, Dave
YiEngr, MA/NY DDave

-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-------------------------------------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2