Hi,
There is a Copper Erosion session at SMTAI next week on Tuesday at
10:00am. Discussion is about rework and lead free HASL w/ nickel as a
surface finish. They will be showing erosion data primarily for rework of
hand and fountain but I'm sure there will be a lively Q&A.
Best regards,
CP
Please respond to "(Leadfree Electronics Assembly Forum)"
<[log in to unmask]>; Please respond to John Burke <[log in to unmask]>
Sent by: Leadfree <[log in to unmask]>
To: [log in to unmask]
cc:
Subject: [LF] FW: [TN] Dissolving copper hole wall using lead free HASL?
HI,
This thread came out in Technet. I am sending it out to leadfree, SMART,
and
RoHSUSAPushback to see if there are any engineers out there that have data
on copper thickness reduction of via hole wall on wave soldering, re-work
etc.
Jasbir, could you send me a copy of your presentation please.
John
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Whittaker, Dewey
(EHCOE)
Sent: Thursday, September 21, 2006 9:57 AM
To: [log in to unmask]
Subject: Re: [TN] Dissolving copper hole wall using lead free HASL?
That's correct. We are gathering a lot of data to support the premise
that SAC soldering of Copper PTHs is a no-no.
Dewey
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dennis Fritz
Sent: Thursday, September 21, 2006 9:49 AM
To: [log in to unmask]
Subject: Re: [TN] Dissolving copper hole wall using lead free HASL?
Well, it stripped out the "cut and paste" from the pdf of Jasbir's slide
at
IPC. Here is what he said on the slide:
During rework with SnAgCu alloy with copper from the PCB: copper
dissolves
with increasing contact time.
Experience: PTH barrel knee erosion after 20 seconds of solder pot
dwell time
Copper dissolution is a function of original barrel/pad thickness,
solder
temperature and alloy (tin percentage), dwell/contact time and solder
flow rate
and type of copper plating.
Studies are ongoing with dissolution rate comparison with various
lead-free
solder alloys and process optimization.
Denny Fritz
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
-------------------------------------------------------------------------------Leadfee
Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send:
SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-------------------------------------------------------------------------------
-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-------------------------------------------------------------------------------
|