Buenos días,
Appendix A, # f of J-STD-001C said "Tip transient voltages generated by
soldering equipment should not exceed 2V peak". My question is: How do you
verify this?
We have a soldering iron tester that met the old MIL-STD-2000A. That is,
we can measure the tip to ground voltage (2 mV RMS max.)
Thank you in advance.
Juan T. Marugan