TECHNET Archives

September 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
X-To:
Date:
Fri, 8 Sep 2006 01:40:18 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, li na <[log in to unmask]>
Subject:
From:
In-Reply-To:
Content-Type:
text/plain; charset=gb2312; format=flowed
Parts/Attachments:
text/plain (50 lines)
Hello Werner,

We measured the resistance at room temperatures after 250, 500, 750 and
1000cycles seperately.  However we did an addtional thermal cylce test to
monitor the real time resistance, the resistance change was still within
spec, this took temperatue affected resistance increase into consideration.
 We also did another 1000 cycle test on the previous test finished
boards(i.e total 2000 cycle test on the daisy boards), the resistance
change measured after 250,500,750 and 1000cycles at room temperature was
still within 10%.  It is really magic to me.  I don't know what to do next
and if there is a high risk to accept the test result.

Thanks.
Lina


>From: [log in to unmask]
>To: [log in to unmask], [log in to unmask]
>Subject: Re: [TN] PTH barrel crack
>Date: Thu, 7 Sep 2006 13:24:35 EDT
>
>Hi Lina,
>I bet you did not monitor in-situ continuously鈥攖hat is an absolute MUST!
At
>RT fully cracked barrels make nice electrical contact, just like
connectors,
>and electrically you never see it.
>
>Regards,
>Werner Engelmaier
>Engelmaier Associates, L.C.
>Electronic Packaging, Interconnection and Reliability Consulting
>7 Jasmine Run
>Ormond Beach, FL 32174 USA
>Phone: 386-437-8747, Cell: 386-316-5904
>E-mail: [log in to unmask], Website: www.engelmaier.com

_________________________________________________________________
享用世界上最大的电子邮件系统— MSN Hotmail。  http://www.hotmail.com

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2