TECHNET Archives

September 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Stadem, Richard D." <[log in to unmask]>
Date:
Mon, 18 Sep 2006 08:10:14 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Whittaker, Dewey (EHCOE)" <[log in to unmask]>
Subject:
From:
"Whittaker, Dewey (EHCOE)" <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (91 lines)
You get an A plus. Perfect tense and syntax. That's exactly the response
I would have given. 
Many of us were at the IPC meetings and we discussed this issue. No one
would believe it was PbCO3. Pure lead needle crystals do to stress or an
imbalance is more understandable, but still pretty amazing.
Dewey

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Wednesday, September 13, 2006 5:23 AM
To: [log in to unmask]
Subject: Re: [TN] PbCO3

Well, I don't think you are losing it, Ioan. I have seen a lot of creeps
with whiskers in this business myself.
Dewey, this is my thesis submission for Friday 101. 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Tempea, Ioan
Sent: Wednesday, September 13, 2006 7:12 AM
To: [log in to unmask]
Subject: Re: [TN] PbCO3

Inge,

I will risk myself and through in some confusion.

How did you realize you had this problem, in the first place? Are you
sure it could produce failures?

Now the slippery teritory, since it's been years since I took my
materials stress class: if I remember well, the stress class we had was
based on several hypoteses and one of them was the homogeneous material.
So the von Mise's I have studied was based on the same material all over
the place. Here you deal with one alloy for the ball, one alloy for the
top attachment and another alloy for the bottom attachment. Maybe this
alters the stress distribution?

Are the whiskers you see mono crystals? In order for you to repeatedly
get them, it is obvious you have the same stress, at the same place,
every time. Maybe you have a Sn starvation at the equator due to
migration towards the joined zones. Then you might have different stress
distributions on the various zones due to different alloys. And on top
of it, the creep. Wouldn't the whiskers a result of the creep?

If you think I am losing it, just have me recall the message.

Regards,

Ioan

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2