TECHNET Archives

September 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Wed, 13 Sep 2006 17:36:32 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Franklin D Asbell <[log in to unmask]>
Subject:
From:
Franklin D Asbell <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (241 lines)
So you're not talking then about a bare board at $50,000.000 as wrote below,
but a populated one...yes?

I can accept a few very specialized, isolated designs, when fully populated
reaching the 50k level, but not a bare board.

Franklin

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Wednesday, September 13, 2006 1:48 PM
To: [log in to unmask]
Subject: Re: [TN] Delamination

I did not say GD built these types of costly boards. I simply stated that
many companies are.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of John Burke
Sent: Wednesday, September 13, 2006 12:54 PM
To: [log in to unmask]
Subject: Re: [TN] Delamination

50K..........??

With a component BOM I hope....................

If it's 50K without, you might as well machine each one out of
solid...............8-)

John

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Franklin D Asbell
Sent: Wednesday, September 13, 2006 10:25 AM
To: [log in to unmask]
Subject: Re: [TN] Delamination

Richard,

MIL-P[RF]-55110/50884/31032 documents clearly state "no repair", of course
if these are military product built to IPC-6010 series then repair may be
performed I agree repair is allowed.

Many OEMs such as Raytheon, LMCO, Boeing, provide PCB suppliers with PCB
Fabrication or Acceptance Specifications which state the same (no repair, or
repair with prior communication), I've reviewed many of these and have had
to comply with these requirements.

I don't disagree that there are many OEMs which would accept this particular
repair (repaired delamination) But in my experience over the past 10 years
I've not seen one of my customers even consider discussing repairing
delaminated product, and as mentioned, today I would not even entertain the
idea of asking them.

Did you say you're building PCB's costing $50,000.00...wow, I'm impressed,
I'm now interested in the design you're building? What material type, layer
count, features, etc. If it does not violate any proprietary of NDA of
course.

Franklin

-----Original Message-----
From: Stadem, Richard D. [mailto:[log in to unmask]]
Sent: Wednesday, September 13, 2006 11:49 AM
To: TechNet E-Mail Forum; Franklin D Asbell
Subject: RE: [TN] Delamination

Wrong, Franklin.

Nearly all medical, industrial, aerospace, military, and government agencies
recognize that qualified repair processes, including for delamination, are
perfectly reliable, in most cases even more reliable than the original
undamaged hardware. There is no more risk in performing a certified repair
procedure than there is in doing standard rework.
That is the reason MRB boards exist in large military OEMs and CEMs such as
Honeywell, Rockwell, GD, etc., etc., with documented, qualified, and
certified repair procedures, non-conforming material segregation and
handling methods, trained and certified operators and inspectors,
traceability systems, and quality departments.
Many of these companies recognize the incidential value in these systems,
including the impact of not having to delay a program, re-order new parts,
re-inspect new parts and boards, re-stock replacement parts and boards,
re-assemble replacement assemblies, re-test, etc, etc.
Simply scrapping a board because it is delaminated may be acceptable for
your product, but many programs cannot afford to scrap a single bare pwb
valued at $50,000 for example, let alone a finished assembly valued at more
than $500,000 because it has a delamination or other repairable defect. And
yes, pwbs and assemblies with those values are becoming somewhat common in
the industry today, what with the rapidly escalating level of technology.
And in most cases, by the time you add up the cost of all of the above
replacement activity, the real hidden cost of scrap becomes a factor in even
the least costly commercial, high-volume products.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Franklin D Asbell
Sent: Wednesday, September 13, 2006 11:23 AM
To: [log in to unmask]
Subject: Re: [TN] Delamination

I'm curious what customers would actually accept repaired delaminated
product.

I read repair procedures for delaminated conditions many years ago and in my
opinion the end result presents many reliability possibilities.

When I see delamination, I see scrap.

Franklin

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Tuesday, September 12, 2006 1:22 PM
To: [log in to unmask]
Subject: Re: [TN] Delamination

Helena, I forgot to mention that many delaminations are quite repairable.
There are repair procedures outlined in IPC-STD-7711/7721.
They are not automatic scrap. This requires MRB authority from your
customer, however.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Pasquito, Helena
Sent: Tuesday, September 12, 2006 11:45 AM
To: [log in to unmask]
Subject: [TN] Delamination

Hi TechNetters,

Let me ask a question; I know delamination is bad, but why?  What is the
failure mode to the board when a board delaminates and would there ever be
an instance that a board that delaminates is still OK to use?  This is a
Class 3 application.  Yes, I know what the IPC standards say but not real
sure about the board process.  Yes, I "googled" and there is a lot of stuff
out there.  Maybe someone can recommend some reading material (hopefully
short and sweet and to the point).

Thanks!
Helena

Helena Pasquito
Manufacturing Skills Instructor
M/A-COM, Tyco Electronics
1011 Pawtucket Blvd., M/S 107
Lowell, MA 01853
978-442-5024
[log in to unmask]


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please visit
IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per
day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please visit
IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per
day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please visit
IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2