TECHNET Archives

September 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="iso-8859-1"
Sender:
Subject:
From:
John Foster <[log in to unmask]>
Date:
Fri, 8 Sep 2006 07:57:07 -0700
MIME-Version:
1.0
X-To:
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (178 lines)
Oh my god the atomic bomb tantalum is fantastic.

How funny.


-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Steve Gregory
Sent: Friday, September 08, 2006 7:50 AM
To: [log in to unmask]
Subject: Re: [TN] Tantalum Caps


Hi Dave!

Yes it's FRIDAY!! (Thank goodness!!) I got your picture and it's posted.
Pretty "dramatic" all right...looks like the thing turned itself inside
out! check out:

http://stevezeva.homestead.com/files/Daves_Tantalum.jpg

I had another picture sent to me that's just as "dramatic". But I think
that this one shorted somehow or was put on backwards...almost blew the
traces off the board! Look at this one:

http://stevezeva.homestead.com/files/Crispy_Tantalum.jpg

Then there's another picture. This one is almost beyond
desciption...check out:

http://stevezeva.homestead.com/files/Real_Crispy_Tantalum.jpg

I wouldn't want to even be around that one, that's for sure!

-Steve Gregory-

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman
Sent: Friday, September 08, 2006 7:35 AM
To: [log in to unmask]
Subject: Re: [TN] Tantalum Caps

Hi Steve! It must be Friday if we are discussing exploding components!
Kemet has an very good summary of what can happen to Ta capacitors - in
short they can have a self sustaining metal oxide fire! Here is the
Kemet
reference: Kemet Electronics Corporation Tantalum Applications Notes,
Surge Step Stress Testing in Tantalum Capacitors, 05/03/00. And I'll
send you a much more "dramatic" photo to post! All components have
limits and Ta caps are no exception.

Dave Hillman
Rockwell Collins
[log in to unmask]




             stephen gregory
             <stephengregory58
             [log in to unmask]>
To
             Sent by: TechNet          [log in to unmask]
             <[log in to unmask]>
cc


Subject
             09/07/2006 06:17          Re: [TN] Tantalum Caps
             PM


             Please respond to
              TechNet E-Mail
                   Forum
             <[log in to unmask]>
             ; Please respond
                    to
              stephen gregory
             <stephengregory58
             [log in to unmask]>






Hi John!

  Certanly can! They can literally EXPLODE!! I have a graphic example of
that with a picture that was sent to me some time ago when I asked about
Tantalums being moisture sensitive. Check out:

  http://stevezeva.homestead.com/files/Rpt_Molded_Tant.jpg

  This is what a tantalum looked like after it came out of reflow!!

  -Steve Gregory-

John Foster <[log in to unmask]> wrote:
  Can Tantalum Caps suffer from popcorning?

Can tant caps absorb enough moisture to cause this type of effect.

We just built some new boards and we have one particular part number
tant that is shorting out left and right.

any input will be appreciated thanks

John Foster

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2