I won't answer your question but both products contain HFCs which have
high global-warming potentials (300-1000 x worse than CO2). They also
contain trans-DCE which is quite a toxic chlorinated solvent and at
least one of them contains methanol which is also a neurotoxin. IMHO,
they should be used only in a properly ventilated hood equipped with a
carbon filter, operators suitably protected and trained (including
proper maintenance and disposal of the carbon filter to prevent
re-emission of the solvents).
Brian
Diamond, Pat wrote:
> Hi all,
>
> has anyone had any experience using a couple of flux removing solvents?
>
> Micro Care Flux Remover C
>
> Techspray Flux remover G3
>
> we are evaluating these hand cleaning solvents to replace our present one.
>
> Or if you have experience of any other alternative cleaners that you think
> might offer better flux removing properties...........
>
> regards,
>
> Pat Diamond
>
> ****************************************************************************
> ***************
> The information transmitted is intended only for the person or entity to
> which it is addressed and may contain confidential and/or privileged
> material.
>
> Any review, retransmission, dissemination or other use of, or taking of any
> action in reliance upon, this information by persons or entities other than
> the intended recipient is prohibited. If you received this in error, please
> contact the sender and delete the material from any computer.
> ****************************************************************************
> ***************
> Mr Pat Diamond
> Senior Specialist Engineer
> Weston Aerospace Tel: +44 (0)1252 868122
> 124 Victoria Road Fax: +44 (0)1252 370298
> Farnborough, Hampshire, GU14 7PW Web www.westonaero.com>
> England Email mailto:[log in to unmask]
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
--
http://www.cypenv.org Cyprus environment/energy
http://www.cypenv.org/worldenv World environment/energy
http://www.cypenv.org/weather Cyprus weather
http://www.cypenv.org/smf/index.php Environment/energy forums
http://groups.yahoo.com/group/cypnature/ Cyprus nature forum
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|