TECHNET Archives

August 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Ingemar Hernefjord (KC/EMW)" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Ingemar Hernefjord (KC/EMW)
Date:
Thu, 31 Aug 2006 10:20:47 +0200
Content-Type:
text/plain
Parts/Attachments:
text/plain (29 lines)
 
We got lots of such growth on CBGA balls recently. After
soldering/cleaning: nada. After one week in stock: signs of growth.
After one month: unacceptable crystals. Now, being insoluble in water
and many solvents, some specialists advise you to mix an RA with
ethanol, heat this mixture and dip the part until the crystals vanish.
My question to TN is whether there is alternative methods? Some accept
PbCO3 growth as being harmless, but this is not our intention, because
loose particles are semiconducting and can create leakage current paths.

Brian's book "Cleaning and Contamination of Electronics and Assemblies"
mention there are five groups of white residues, but, oddly enough, lead
carbonate is not included. The chemistry world of soldering residues is
so complicated, that I have to ask you for help.

Thanks in advance
Ingemar Hernefjord
Ericsson Microwave Systems

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2