Hi, Mr. Engelmair and other Netters
What does STII stand for?
It looks like a measurement of thermal stability.
I know T260 or T288 but not STII.
I just want to know since IĄ¯ve been in this material business for some time.
And I hope I am not the only one who doesnĄ¯t know what STII is.
Many thanks in advance.
Tim (Minsu) Lee
Technical Marketing
Doosan Electro-Materials
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner Engelmaier
Sent: Wednesday, August 23, 2006 6:45 AM
To: [log in to unmask]
Subject: Re: [TN] N4000-29 material
Hi Ted,
Here are the pertinent fact about the materials:
Isola IS410 Tg=170, Td=350, TE(50->260)=3.5%, STII=225
Nelco N4000-11 Tg=170, Td=345, TE(50->260)=3.2%, STII=225 Nelco N4000-12 Tg=180, Td=370, TE(50->260)=3.6%, STII=239
N4000-29 Tg=175, Td=350, TE(50->260)=3.0%, STII=232
Generally, the higher the STII the better the material is for LF-soldering temperatures.
Werner
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|