True, silver is a lower cost to a board shop who has both lines. But if a
customer has a supplier spec'ed in who only has ENIG, the cost to the
customer will be the same due to the supplier having to sub-contract out, or
they spec in another supplier who has both, or work with the supplier to
commit work to support the new line.
Chad
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jeffrey Bush
Sent: Tuesday, 15 August 2006 10:23 PM
To: [log in to unmask]
Subject: Re: [TN] Immersion Au vs Immersion Ag
Silver is by far lower cost than ENIG - materials, process and space needed
to maintain a line. Deposition processes are high maintenance and need to
be run day to day. Having to keep this line loaded with panels influences
my view of ENIG performance internally and in the field.
Jeffrey Bush
Director, Quality Assurance and Technical Support VERMONT CIRCUITS
INCORPORATED
76 Technology Drive - POB 1890
Brattleboro, Vermont 05302
Voice - 802.257.4571 ext 21
Fax - 802.257.0011
<http://www.vtcircuits.com/>
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of John Parsons
Sent: Monday, August 14, 2006 5:59 PM
To: [log in to unmask]
Subject: Re: [TN] Immerison Au vs Immersion Ag
The "price" would depend on the source. If your favorite fabricator does
not have an in-house Ag line then ENIG may be cheaper or vice versa. If
they have both then, yes, Ag is likely cheaper.
John
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Chad Renando
Sent: Monday, August 14, 2006 2:55 PM
To: [log in to unmask]
Subject: Re: [TN] Immerison Au vs Immersion Ag
I am hearing a lot of discussion about reliability and compatibility.
From
the sounds of it, it seems to be a wash. If that is the case, from a
commodity perspective, I would think you would get a cheaper price for
silver, so if shelf life is not an issue, why not go with that?
Chad
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dave Seymour
Sent: Tuesday, 15 August 2006 3:33 AM
To: [log in to unmask]
Subject: [TN] Immerison Au vs Immersion Ag
We are having a little talk about surface finish for RoHS compliance.
We have been doing Immersion Gold for 10+ years and are starting to switch
to Immersion Silver because some feel that Silver is a better finish for
RoHS compliance.
I can't find anything that says one can not be compliant with Immersion Gold
and I'm trying to figure out why the surface finish should change at all.
Could someone point to some articles, opinions or sources that might help
resolve the issue?
I'm out doing some web looking now.
Thanks
Dave
--
Dave Seymour, CID+
Catapult Communications Inc.
800 Perimeter Park Dr, Suite A
Morrisville, NC 27560
Direct: (919)653-4249
Main: (919)653-4180
Fax: (919)653-4297
[log in to unmask]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per
day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per
day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information,
or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|