Jeff,
Just to make sure that I read your reply correctly - should I infer from
your comments that you believe the IAg process 'likes' to have a
round-the- clock, steady-state flow to keep it stable and that the ENIG
process does not? Or did you mean it the other way around, that the
ENIG likes round-the-clock operation?
Am not all that intimately familiar with either line and did not wish to
"read in" something that was not intended.
Steve
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jeffrey Bush
Sent: Tuesday, August 15, 2006 8:23 AM
To: [log in to unmask]
Subject: Re: [TN] Immersion Au vs Immersion Ag
Silver is by far lower cost than ENIG - materials, process and space
needed to maintain a line. Deposition processes are high maintenance
and need to be run day to day. Having to keep this line loaded with
panels influences my view of ENIG performance internally and in the
field.
Jeffrey Bush
Director, Quality Assurance and Technical Support
VERMONT CIRCUITS INCORPORATED
76 Technology Drive - POB 1890
Brattleboro, Vermont 05302
Voice - 802.257.4571 ext 21
Fax - 802.257.0011
<http://www.vtcircuits.com/>
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of John Parsons
Sent: Monday, August 14, 2006 5:59 PM
To: [log in to unmask]
Subject: Re: [TN] Immerison Au vs Immersion Ag
The "price" would depend on the source. If your favorite fabricator
does
not have an in-house Ag line then ENIG may be cheaper or vice versa. If
they have both then, yes, Ag is likely cheaper.
John
THE INFORMATION CONTAINED IN THIS E-MAIL MESSAGE AND ANY ATTACHMENTS SENT FROM GENTEX CORPORATION IS GENTEX CONFIDENTIAL INFORMATION INTENDED ONLY FOR THE PERSONAL USE OF THE INDIVIDUAL OR ENTITY NAMED ABOVE. If you are not the intended recipient, you are hereby notified that any review, distribution, or copying of this communication is strictly prohibited. If you have received this communication in error, please immediately notify the sender by return e-mail, and delete this e-mail message and any attachments from your computer.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|