Hi George,
The 3% silver in SAC305 are uniformly distributed throughout the solder
joint; the Ag from surface treatments typically concentrates near the
interfaces.
Werner
-----Original Message-----
From: [log in to unmask]
To: [log in to unmask]
Sent: Fri, 11 Aug 2006 12:17 PM
Subject: Re: [TN] silver embrittlement
Sue,
You have every right to be confused, as the chairman of the plating
committee that put out the specification 4553, I have gone back and
re-read the
specs. The specs refer to thin silver and thick silver.
My apologies for the poor choice of terminology, the intent was to
differentiate between the Alpha Level product which could only produce
a very
thin
coating and the rest of the Immersion silvers out there that could
produce a
thicker coating. So "thin" is a spec for Alpha level only and the
"thick" is
the
spec for all other immersion silvers.
For users not specifying Alpha Level the spec is:
5 uins minimum, typical 8uins-12uins.
Thick silver would be silver at 20uins or higher.
Thicker silver is unnecessary and may give rise to compromised solder
joint
strength. I am not sure that embrittlement is the main defect here,
after all
the Pb/free SAC 305 alloy contains 3% silver.
George Milad
(Chairman IPC Plating Committee)
National Accounts Manager for Technology
Uyemura International Corp (UIC)
249 Town Line Rd
Southington CT 06489
[log in to unmask]
Cell: (516) 901 3874
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
________________________________________________________________________
Check out AOL.com today. Breaking news, video search, pictures, email
and IM. All on demand. Always Free.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|