TECHNET Archives

August 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 18 Aug 2006 19:18:16 +0100
Reply-To:
Subject:
From:
Mike Fenner <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
<002e01c6c2d4$de6f76e0$67058484@KEVINGLIDDEN>
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (112 lines)
Brass is zinc and copper so if you suck out the zinc -dezincification - you
will end up with just the copper, and that is what you are seeing. As you
say the mechanism is diffusion of Zinc into the tin of the solder so is not
flux related (save that the solder has to wet the brass for it to happen,
which it won't do in the absence of flux, at least not very well).
Potentially there are structural problems in the joint area associated with
this and you will also be dumping zinc into your solder pot if you're using
one, not desirable. The zinc will make oxide skin and can also cause grainy
or lumpy joints if allowed to accumulate.
You should specify "immunised" brass, this means the brass is plated with
copper or nickel before tinning, so the solder does not see the brass. This
is a standard procedure/finish and should not present any supply issues.


Regards

Mike Fenner
Indium Corporation

T: + 44 1908 580 400
M: + 44 7810 526 317
F: + 44 1908 580 411
E: [log in to unmask]
W: www.indium.com
Pb-free: www.Pb-Free.com



-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Kevin Glidden
Sent: Friday, August 18, 2006 3:45 PM
To: [log in to unmask]
Subject: [TN] Soldering to brass

A metallurgist I am not....

We have brass eyelets that we solder wires into.  I am unable to obtain
detailed information on the specific alloy, but the vendor told me it was
70% Copper, 30% Zinc.  We are soldering using 63/37 solder and RMA flux.
During soldering, the eyelet appears to change to copper in the non-soldered
areas.  A brief search of some Tech-Net archives has told me that the Zn
will diffuse out and create solderability problems.  But is the end result
that the material appears to be copper as in my case?

As a side note, I tried a water sol flux and observed the same condition.  I
then tried simply heating an eyelet with an iron - no flux or solder - and
there was no change, so it appears to be flux related.  I also cut a piece
up to verify it is solid brass, not plated.  We tried brushing the eyelet
after soldering and it appears that you can restore the brass finish to some
extend.

Anyway, I have confirmed with the supplier these should have been hot solder
dipped, and we have already ordered replacements.  But I am now faced with a
question I cannot answer - what is the reliability concern of this
phenomenon, if any?  These solder joints get conformal coated, and then the
entire PCB is RTV'd into a case, so it is well sealed.  Can I continue to
use the existing stock, or is this a serious reliability issue?

Thanks!




Kevin Glidden

Manufacturing Engineer



Astronics Luminescent Systems Inc.

4 Lucent Drive

Lebanon, NH 03766



P: 603-643-7766 x3152

F: 603-643-5947



---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------


***This email, its content and any files transmitted with it are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient please delete and contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon, this information by persons or entities other than the intended recipient is prohibited.

Messages sent via this medium may be subject to delays, non-delivery and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. In particular, Indium Corporation does not accept responsibility for changes made to this email after it was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.***

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2