Hi Kerry,
The direct cause is a separation force too large for the adhsion present.
Now, there are three underlying reasons that could be individually
responsible or acting in combination: (1) low quality, (2) bad design/material choices,
and (3) loads higher than normal [whatever normal is].
(1) Most of the responses so far have dealt quite adequately with 'low
quality' issues.
(2) You have indicated FR-4 with Tg=170 [which is good if measured by TMA],
but you say nothing about CTE's and Td—which are very important in this
context. You indicated that you saw thin Cu barrel plating—that will cause excessive
expansion of the resin into the hole space causing plastic deformation of the
Cu plating—on cooling, it simply cannot come back to its former geometry. It
will depend on how thin the Cu actually is and whether or not you have removed
non-functional lands [You may want to check out my Reliability Column in
Global SMT & Packaging magazine, August 2006 issue]. You are actually lucky that
you did not see barrel cracking under the circumstances [depends on drilled hole
diameter, of course]. I am dealing with many of these issues in my recent
White Paper on the changes needed for PCB FAB notes and specifications for
lead-free soldering [I will send the nfo by separate mail]
(3) Higher loads are certainly being generated with the higher lead-free
soldering temperatures. You also could get higher loads with entraped moisture
creating excessive internal vapor pressure.
Regards,
Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL 32174 USA
Phone: 386-437-8747, Fax: 386-437-8737, Cell: 386-316-5904
E-mail: [log in to unmask], Website: www.engelmaier.com
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|