TECHNET Archives

August 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Creswick, Steven" <[log in to unmask]>
Date:
Tue, 15 Aug 2006 11:04:49 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, R Sedlak <[log in to unmask]>
Subject:
From:
R Sedlak <[log in to unmask]>
Content-Transfer-Encoding:
8bit
In-Reply-To:
Content-Type:
text/plain; charset=iso-8859-1
MIME-Version:
1.0
Parts/Attachments:
text/plain (36 lines)
To review, what I have discussed perhaps too many times...

  When you plate metals, you transfer electrons to the ions in solution, turning the ions into metal.
  There are three kinds of plating from an electrolyte, Electrolytic, Electroless and Immersion... they differ primarily in where the electrons which cause plating come from.

  In Electrolytic, the electrons are "pumped" from the anode to the work by the rectifier.

  In Electroless, the electrons are supplied by another chemical in the electrolyte, like Formaldehyde (electroless Copper) or Hypophosphite (Electroless Nickel).

  In Immersion plating, the electrons are supplied by the substrate (usually Copper in our world) as it goes into solution.

  In general, any immersion plating bath is easier to maintain/control and thus get good plating from, than an electroless plating bath, as there is so much less to worry about.

  So ENIG, although it may give a superior finish, when done right, is one difficult bath to have work correctly, and frankly, my hat is off to those of you who have mastered this process, I am glad I do not have to do this....and make money from the process too.

  Think of it this way, it is possible to walk away from most immersion baths, for days, return, turn on the heat, and plate.... this is rarely the case with an electroless bath.

  Rudy Sedlak
  RD Chemical Company




---------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
Yahoo! Messenger with Voice. Make PC-to-Phone Calls to the US (and 30+ countries) for 2¢/min or less.

ATOM RSS1 RSS2