Dear Experts,
IEC TC111 section 9 describes ISO 3613:2000(E) as the method to be
adopted for determining Cr6 on metallic samples. IEC TC111 section 10
describes EPA 3060A & EPA 3060A as the method to be adopted for
determining Cr6 on polymer materials and electronic compounds.
For the USB cables which method is to be adapted for Cr6
determination? I guess below are the homogenous parts for a cable or is
there a big list of homogenous parts in a cable?
1. The sheathing material used as insulation
2. The conductor.
3. The braid used for shielding.
Sincerely
K.Balasubramanian
Project Leader - Hardware.
-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-------------------------------------------------------------------------------