Not sure about using silver as a contact finish, the oxides are conductive,
the sulphides - I don't think so, I have seen no studies either on "number
of contacts to failure data".
I do know that when I tried this back in the summer of 1996 on the keyboards
of PSION organizers when I was running that plant, that the keyboards on
some of the proto type units stopped working after a month.
John
-----Original Message-----
From: Leadfree [mailto:[log in to unmask]] On Behalf Of Lester Subrattee
Sent: Friday, August 18, 2006 8:07 AM
To: [log in to unmask]
Subject: Re: [LF] Immersion Silver and Conductive Carbon Ink
Hi Scott,
I don't have a solution for your problem except to say that you're
depositing on metal and should have no issues if it is clean. Unless the
silver is actually lifting off. I think it could be a surface prep issue or
contamination from either the PCB house or your fabricator in handling. Get
the surface analyzed and cleaned, then retry.
That being said, there have been studies by some OEMs that indicate
capability of Immersion Silver as a contactable surface in lieu of gold.
That is one of the reasons Immersion Silver's popularity has increased.
Unfortunately, I don't have the details and reports but someone on the Forum
might.
Good Luck,
LS
-----Original Message-----
From: Douglas, Scott [mailto:[log in to unmask]]
Sent: Friday, August 18, 2006 10:41 AM
To: [log in to unmask]
Subject: Immersion Silver and Conductive Carbon Ink
Fellow list persons,
=20
I have a printed circuit board used in a remote control unit. We changed
the solder plating on the board to immersion silver for RoHS compliance.
Our fabricator is having a problem getting the conductive carbon ink to
stick to the immersion silver. Is anyone aware of this type of problem?
We are trying to figure out if we just have a vendor problem or is there
some issue with the immersion silver and conductive carbon ink
combination. Any suggestions as to changes or corrective actions?
=20
As always, thank you in advance for your comments.
Scott Douglas, NCE=20
Staff Technical Specialist
Harman Specialty Group=20
3 Oak Park Drive=20
Bedford, MA 01730=20
Phone: (781) 280-0406=20
Email: [log in to unmask]
Web: www.harmanspecialtygroup.com=20
----------------------------------------------------------------------------
---Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send:
SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=3D4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
----------------------------------------------------------------------------
---
THIS EMAIL AND ANY ATTACHED FILES ARE CONFIDENTIAL AND MAY BE LEGALLY
PRIVILEGED. If you are not the addressee, any disclosure, reproduction,
copying, distribution or other dissemination or use of this communication is
strictly prohibited. If you have received this transmission in error, please
notify the sender immediately and delete this email. It is the policy of ACR
Electronics, Inc. that no legally binding statements, representations or
commitments (collectively statements) may be made by email. Any such
statements must be confirmed either by facsimile transmission or by postal
mail before they will have legal effect. The sender of this email is not
authorised to commit the company in any way and the addressee is hereby
notified of that fact.
----------------------------------------------------------------------------
---Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send:
SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
----------------------------------------------------------------------------
---
-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-------------------------------------------------------------------------------
|