Paul
the IC is either compliant or not...I think I smell the old "lead weight"
in the product coming up where people add up the actual lead content
regardless of it homogeneous content
advice 1: plenty of labs around for test, Sodertec is one (AKA Tin
Technology)
advice 2 : if the IC has "tin/lead" solder on legs, get it stripped and
re-plated with matte tin, again there are people that do this in the UK
regards
Paul
Paul R Taylor
Senior Engineer, RoHS Compliancy Group, IED
Pitney Bowes Ltd
The Pinnacles, Elizabeth Way, Harlow, Essex, CM19 5BD
tel: +44 1279 449 744 fax +44 1279 449 594
email: [log in to unmask] website: www.pb.com
Paul Jackson <[log in to unmask]>
Sent by: Leadfree <[log in to unmask]>
14/08/2006 13:32
Please respond to
"(Leadfree Electronics Assembly Forum)" <[log in to unmask]>; Please respond
to
Paul Jackson <[log in to unmask]>
To
[log in to unmask]
cc
Subject
[LF] Testing resource
One of my manufacturing plants is in a quandary over the following
The are not sure about the limits per product.. If there are two chipsets
in a product and both are over the RoHS limit together but not
individually how is it tally up....as they are x2 in a product and x3 in
another.... also is there anywhere in the Uk that are able to test
products that wont cost a huge amount,,,>
Paul Jackson
Hotline Purchasing Manager
Black Box Network Services
Tel: 0118 965 5225
Fax: 0118 9751 565
E-Mail: Paul <mailto:[log in to unmask]> [log in to unmask]
Web: www.blackbox.co.uk
One source for worldwide infrastructure services
*********************************************************************************
One source for worldwide infrastructure services
Black Box is the world's largest technical services company dedicated to
designing, building and maintaining today's complicated network
infrastructure systems.
Black Box services clients of all sizes in 141 countries throughout the
world.
This email and any files transmitted with it are confidential and intended
solely for the use of the individual or entity to whom they are addressed.
If you have received this email in error please notify the sender by
replying to this email.
This footnote also confirms that this email message has been swept by
MIMEsweeper for the presence of computer viruses.
www.blackbox.co.uk
*********************************************************************************
-------------------------------------------------------------------------------Leadfee
Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send:
SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-------------------------------------------------------------------------------
-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-------------------------------------------------------------------------------
|
|
|