My understanding is lead is generally added for machining aluminum.
Here is a short article summarizing lead use in 2002
http://www.secat.net/answers_view_article.php?article=New_Alloys_Get_the
_Lead_Out_of_Free-Machining_Aluminum.html
Also. From
http://www.key-to-metals.com/Article55.htm
Lead. Normally present only as a trace element in commercial-purity
aluminum, lead is added at about the 0.5% level with the same amount as
bismuth in some alloys (2011 and 6262) to improve machinability.
Dan Kallin
Phone: 978.371.4155 Fax: 978.371.2468
Mobile: 978.760.0779
[log in to unmask]
-----Original Message-----
From: Leadfree [mailto:[log in to unmask]] On Behalf Of Genny Gibbard
Sent: Thursday, August 10, 2006 1:32 PM
To: [log in to unmask]
Subject: [LF] Metal compliance
Anyone else having major difficulties getting RoHS compliance statements
out of your metalwork suppliers?
We have companies that provide things like chassis parts, custom
standoffs, etc. They are made of things like 6061 Aluminum, stainless
steel, etc. These are things that can use the exemption:
6. Lead as an alloying element in steel containing up to 0.35 % lead by
weight, aluminium containing up to 0.4 % lead by weight and as a copper
alloy containing up to 4 % lead by weight.
However, our metalwork vendors are having trouble getting any sort of
statement out of their raw materials suppliers, so they are reluctant to
issue statements to us.
I don't know if it would be an unlikely thing to have higher than the
0.4% Pb in aluminum, or if you need to have some carefully controlled
source of aluminum in order to achieve that.
Any thoughts?
As always, your help is much valued and appreciated.
------------------------------------------------------------------------
-------Leadfee Mail List provided as a service by IPC using LISTSERV
1.8d
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks
send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
------------------------------------------------------------------------
-------
This e-mail is intended to be delivered only to the named addressee(s) and may contain information that is confidential and proprietary. If this
information is received by anyone other than the named addressee(s), the recipient(s) should immediately notify the sender by e-mail and promptly
delete the transmitted material from your computer and server. In no event shall this material be read, used, stored, or retained by anyone other
than the named addressee(s) without the express written consent of the sender or the named addressee(s).
-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-------------------------------------------------------------------------------
|