True, possibly with two exceptions.
SnBi finish may be a problem, depending on the amount
of bismuth. I've seen some studies showing up to
6% Bi in the bulk solder should be OK. There may
additional caveats for Kovar or Alloy 42 leads.
And if you consider BGA balls to be a finish, there are
other things to consider.
-Joe
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Mike Fenner
Sent: Wednesday, August 09, 2006 6:03 PM
To: [log in to unmask]
Subject: Re: [TN] Pb-free backward compatibility matrix
There is no matrix: Lead free finishes are compatible with leaded
solders.
Regards
Mike Fenner
Indium Corporation
T: + 44 1908 580 400
M: + 44 7810 526 317
F: + 44 1908 580 411
E: [log in to unmask]
W: www.indium.com
Pb-free: www.Pb-Free.com
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Macko, Joe @ IEC
Sent: 09 August 2006 15:03
To: [log in to unmask]
Subject: [TN] Pb-free backward compatibility matrix
Good morning fellow TechNet's,
As everyone knows, many smt components now have Pb-free finishes such as
NiPdAu by TI that can still be soldered using leaded solder. Would
someone
please let me know where I can find a cross reference matrix, etc.
showing
the various backward compatible Pb-free finishes that work with leaded
solder and any issues!
Thanks again
Joe
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
***This email, its content and any files transmitted with it are
intended solely for the addressee(s) and may be legally privileged
and/or confidential. If you are not the intended recipient please delete
and contact the sender by return and delete the material from any
computer. Any review, retransmission, dissemination or other use of, or
taking of any action in reliance upon, this information by persons or
entities other than the intended recipient is prohibited.
Messages sent via this medium may be subject to delays, non-delivery and
unauthorized alteration. This email has been prepared using information
believed by the author to be reliable and accurate, but Indium
Corporation makes no warranty as to accuracy or completeness. In
particular, Indium Corporation does not accept responsibility for
changes made to this email after it was sent. Any opinions or
recommendations expressed herein are solely those of the author. They
may be subject to change without notice.***
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|