On the whole, from a quick skim through, I find the doc is intelligible.
The grammar is atrocious in places and the consistency of terminology is
poor. A few hours work by a skilled technical editor would bring it up
to scratch, IMHO.
Brian
Gerard O'Brien wrote:
> Rudy - I would appreciate it when you decide to slam the work of the
> committees that you correctly identify the committee you are having a
> problem with. You say in the first paragraph that you received this message
> pertaining to your negative vote on the immersion tin standard but yet the
> message from Tom pertains to the 003B solderability standard.
> As co-chairman of the committee responsible for the immersion tin standard I
> would like to point out that a) you are not on the mailing list, b) we did
> not receive a negative vote from you.
>
>
> Regards
>
> Gerard O'Brien
> Co-chairman of 4-14
>
>
>
> -----Original Message-----
> From: R Sedlak [mailto:[log in to unmask]]
> Sent: Tuesday, August 29, 2006 9:35 PM
> To: [log in to unmask]
> Subject: [TN] Does anyone else on Technet find this situation beyond
> comprehension?
>
> Just in case anyone still has any remaining hopes that the IPC might
> actually someday attempt to achieve something worthwhile, or perhaps attempt
> to minimize the confusion in our world, I offer this e-mail message which I
> received from the IPC in response to my negative vote on the proposed
> Immersion Tin standards.
>
> It is important to realize, to get the full flavor of this message, that
> the standard was submitted to me for my review with two options: 1. Accept
> as written, or 2. reject, with reasons given for rejection. I rejected,
> because the standard was written in a way which was essentially
> unintelligible, and I could not even figure out what they were trying to
> say.
> I received the following message in return.
>
>
> ---------------------------------
>
> From: Tom Newton [mailto:[log in to unmask]]
> Sent: Tuesday, August 29, 2006 6:46 AM
> To: Rudy Sedlak
> Subject: Your Negative Vote Submitted Against IPC J-STD-003B
>
>
> Rudy Sedlak:
>
> The IPC 5-23a Printed Wiring Board Solderability Specification Task Group
> is in the final stages of resolving all Technical Comments for the initial
> Ballot or potential upcoming Negative Vote Resolution Ballot on IPC
> J-STD-003B, Solderability Tests for Printed Boards document. Sadly, this is
> admittedly a
> very long time since the original Ballot was closed at the end of June
> 2006.
>
> Never-the-less, I am now responding back to you on your Negative Vote
> submitted on June 26, 2006.
>
> Please note that I have attached this response to the full string of
> E-mail correspondence we have had on this document, so that the 'history' of
> these
> communications is recorded.
>
> Your vote on the ballot for IPC J-STD-003B will be shown as having been
> submitted toward the Ballot on IPC J-STD-003B. That is, IPC will show that
> you did reply to the Ballot.
>
> However, because the following statement:
> "The wording is so difficult to understand and convoluted, and it is so
> verbose, it is essentially unintelligible. (And if I am offending key
> people, I apologize, but somebody has to draw a line in the sand.)"
>
> that was provided as your sole support for your Negative Vote does not
> contain at least one specific technical detail with a suggested technical
> solution, your negative vote will not be accepted by the 5-23a Task Group.
>
> This response will be duly recorded with all of the actions concerning the
> IPC Ballot for the IPC J-STD-003B document. Additionally, if IPC has
> communication with the American National Standards Institute (ANSI) on this
> document, your vote will be shown as an "Unsupported Negative Vote" (one of
> ANSI's vote categories).
>
> Accordingly, IPC thanks you for your ballot submission on IPC J-STD-003B.
>
> Sincerely,
>
> Thomas D. Newton
> Director PCB Programs, Standards and Technology
> IPC - Association Connecting Electronics Industries
> 3000 Lakeside Drive; Suite 309-S
> Bannockburn, IL 60015
> Direct: 847-597-2849 Main: 847-615-7100
> Fax: 847-615-7105
> E-mail: [log in to unmask] web: www.ipc.org
>
>
>
>
> ---------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
> How low will we go? Check out Yahoo! Messenger's low PC-to-Phone call
> rates.
>
> This e-mail and any attachments may contain confidential and
> privileged information. If you are not the intended recipient,
> please notify the sender immediately by return e-mail, delete this
> e-mail and destroy any copies. Any dissemination or use of this
> information by a person other than the intended recipient is
> unauthorized and may be illegal.
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
--
http://www.cypenv.org Cyprus environment/energy
http://www.cypenv.org/worldenv World environment/energy
http://www.cypenv.org/weather Cyprus weather
http://www.cypenv.org/smf/index.php Environment/energy forums
http://groups.yahoo.com/group/cypnature/ Cyprus nature forum
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|