TECHNET Archives

August 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Jeffrey Bush <[log in to unmask]>
Date:
Fri, 4 Aug 2006 10:03:03 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Terry Kozlyk <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
Terry Kozlyk <[log in to unmask]>
Parts/Attachments:
text/plain (140 lines)
Any reputable & sound fabrication shop runs ALL the gerber data thru
their VALOR tool ( industry standard ) which flags all sorts of
problems, including this silkscreen on pads issue. Some will just fix it
and not tell you. Others will & let you know about it.

But any fab shop which just prints the gerber data blindly, should not
be one you deal with. Many of them now provide Value Added Service, like
none other, so they will NOT allow garbage like this to go onto their
finished PCB's.

Yes, there are all sorts of fabricators out there, but why do work with
any who isn't reputable & top notch. How much do you really save?

Regards
TDK




-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jeffrey Bush
Sent: Wednesday, May 17, 2006 6:11 AM
To: [log in to unmask]
Subject: Re: [TN] Silkscreen on pads

Many CAD systems have issues with effective reference clipping and I
would estimate more than 1/2 of our clients have the no-silk rule in
either the drawing or a PCB fab spec specification.  We can perform the
clipping more efficiently than most CAD systems and any issues
encountered can be spun back to the designers for verification.

Jeffrey Bush
Director, Quality Assurance and Technical Support
VERMONT CIRCUITS INCORPORATED 
           76 Technology Drive - POB 1890 
              Brattleboro, Vermont 05302
                Voice - 802.257.4571 ext 21
                    Fax - 802.257.0011
                       <http://www.vtcircuits.com/> 
                           
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ted Tontis
Sent: Tuesday, May 16, 2006 4:12 PM
To: [log in to unmask]
Subject: Re: [TN] Silkscreen on pads

        If the customer had silk on the pads in the art work and a
manufacturing note stating, "There shall be no silk screen on exposed
copper", then bare board supplier needs to take responsibility for the
problem. The bare board supplier should have contacted the customer and
said there is a problem, the art work doesn't match the fabrication
notes. That's why fabrication notes need to follow the art work to help
flag the inconsistencies or errors that tend to slip through the cracks.
Lets say the board was produced some place else and the old board
supplier caught it fixed it and didn't say a word, never happens right?
The customer would have never known that there was a problem, how do you
fix a problem you don't know exists? 
	

Ted T.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Chuck Brummer
Sent: Tuesday, May 16, 2006 2:44 PM
To: [log in to unmask]
Subject: Re: [TN] Silkscreen on pads

Rush,


Great response!  Mistakes made by both parties, work together to solve
the
problem and make the situation win/win.

Chuck Brummer
3M Manufacturing Engineer
8357 Canoga Ave.
Canoga Park, CA 91304-2605
(818) 734-4930



------------------------------------------------------------------------
---------------
Confidentiality Notice

This e-mail and any attachment(s) are intended for the individual or
entity to which this email is addressed and may contain information that
is confidential.  If you are not the intended recipient or an employee
or agent responsible for delivering this e-mail to the intended
recipient, please be aware that any dissemination, distribution or
copying of this communication is strictly prohibited.  If you have
received this in error, please notify the sender by telephone at
604.430.4336 or by return e-mail, and please delete or destroy all
copies of this communication.  Thank you!

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2