TECHNET Archives

August 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Fri, 4 Aug 2006 10:07:42 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Neil Maloney <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="US-ASCII"
From:
Neil Maloney <[log in to unmask]>
Parts/Attachments:
text/plain (143 lines)
Our Alphametals guy says that they (Alpha)have never seen this before.
Nobody else in the solder business (machine or material) has an answer
for us either.  I guess that I will buy a few new fingers and see if
they grab solder off the wave.  

-----Original Message-----
From: Eric CHRISTISON [mailto:[log in to unmask]] 
Sent: Friday, August 04, 2006 8:12 AM
To: [log in to unmask]
Subject: Re: [TN] SAC 305 solder on TI wave solder machine transport
fingers


Kevin,

I don't have a solution but I wonder if you've discussed the problem
with the solder manufacturers? They should understand the metallurgy of
their product and hopefully be able to give you a solution.

Regards,



Kevin Glidden wrote:
> You could try buying some composite material (pallet and fixture 
> materials) and having replacement fingers machined for you..expensive 
> solution but it would work...
>
> Kevin Glidden
> Manufacturing Engineer
> Luminescent Systems Inc.
>
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Neil Maloney
> Sent: Thursday, August 03, 2006 5:05 PM
> To: [log in to unmask]
> Subject: [TN] SAC 305 solder on TI wave solder machine transport 
> fingers
>
> Greetings Technet.
>
> I have an interesting problem that has developed since we converted to

> our lead-free process.  We have been using an Electrovert Astrapak for

> our wave solder operation for many years in our SnPb process.  A few 
> months ago, we converted the machine for SAC305 by installing new 
> titanium parts (solderpot, pumps, wave guides, etc) and loaded it up 
> with Alpha metals SAC305. We removed and cleaned up the transport 
> fingers in alcohol while the pot conversion was under way.  After 
> putting the machine back together our new lead-free process seemed 
> perfect -- except that now the SAC305 is sticking to the titanium 
> transport fingers- I mean really sticking to them. The smooth wave 
> doesn't seem to affect the fingers as much as the chip wave- but after

> a run of about 200 PCBs- the fingers are fouled with solder - to the 
> point that we have to stop and brush out the fingers with a rotary 
> wire brush.
>
>
> We never had this problem with leaded solder. We do not have an 
> automatic finger-cleaner installed on the machine (we never had this 
> problem before) and I cannot find one anywhere to retrofit.  But the 
> question still comes down to-- what is causing the solder to stick 
> where it did not stick before?
>
>
> We use a no -clean flux (Alpha EF2202 or Indium 1075, makes no 
> difference --the solder still sticks.) The fingers were not changed 
> out (only soaked and cleaned with alcohol) when the rest of the 
> machine was converted to lead-free.
>
> Any insight into solving the problem would be greatly appreciated.
>
> Neil Maloney, Manufacturing Engineer
> Contemporary Control Systems, inc
> 2431 Curtiss St Downers Grove, IL  60515
> (630) 963-7070 x132
> [log in to unmask]
> http://www.ccontrols.com <http://www.ccontrols.com/> 
> http://www.ctrlink.com <http://www.ctrlink.com/>
>
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e To 
> unsubscribe, send a message to [log in to unmask] with following text in

> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt 
> or
> (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet
> NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
> e-mail to [log in to unmask]: SET Technet Digest Search the archives of
> previous posts at: http://listserv.ipc.org/archives Please visit IPC
web
> site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100
> ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e To 
> unsubscribe, send a message to [log in to unmask] with following text in

> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt 
> or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET

> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the 
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the 
> archives of previous posts at: http://listserv.ipc.org/archives Please

> visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
> -----------------------------------------------------
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2